Deep sub-zero failure behavior of adhesively bonded single-lap joints: experimental and numerical investigation
Journal of the Brazilian Society of Mechanical Sciences and Engineering, cilt.48, sa.13, 2026 (SCI-Expanded, Scopus)
- Yayın Türü: Makale / Tam Makale
- Cilt numarası: 48 Sayı: 13
- Basım Tarihi: 2026
- Doi Numarası: 10.1007/s40430-026-06864-y
- Dergi Adı: Journal of the Brazilian Society of Mechanical Sciences and Engineering
- Derginin Tarandığı İndeksler: Science Citation Index Expanded (SCI-EXPANDED), Scopus, Aerospace Database, Compendex, INSPEC, Materials Science & Engineering Collection (ProQuest), Technology Collection (ProQuest)
- Anahtar Kelimeler: Adhesive bonding, Energy absorption, Fracture energy, Low-temperature, Single-lap joint (SLJ)
- Ankara Yıldırım Beyazıt Üniversitesi Adresli: Evet
Özet
This study investigates the low-temperature performance of adhesively bonded single-lap joints through combined experimental testing and finite element analysis. To address the limited understanding of the coupled effects of temperature and overlap length on SLJ behavior, an integrated experimental–numerical framework is developed for deep sub-zero conditions. SLJs fabricated with a structural epoxy adhesive were subjected to quasi-static tensile loading at room temperature, − 30 °C, and −60 °C using two overlap lengths. Complementary FE simulations were performed in Abaqus, incorporating temperature-dependent adhesive properties and cohesive zone modeling to capture damage initiation and evolution. The numerical predictions showed strong agreement with the experimental load–displacement curves and failure modes. Results indicate that the strain energy release rate decreases significantly at low temperatures—by about 40% at − 30 °C and nearly 50% at − 60 °C—reflecting increased brittleness with decreasing temperature. Despite this reduction, increased adhesive strength at low temperatures leads to a partial compensation effect, resulting in relatively stable energy absorption for a given overlap length. The study further highlights that overlap length is the primary design parameter controlling energy absorption, while thermally induced stresses remain well below the damage-initiation threshold even at − 60 °C. Additionally, low-temperature exposure alone does not initiate damage within the adhesive layer, confirming that failure is governed by mechanical loading rather than thermal mismatch. Overall, the study provides new insights into the coupled roles of temperature, geometry, fracture properties, and thermal stresses, offering practical guidance for the design of bonded joints operating in extreme low-temperature environments.