PITTING CORROSION BEHAVIOUR OF ST 37 STRUCTURAL STEEL IN SEVERAL CORROSIVE ENVIRONMENTS


ÖKTEM M. F., ÇELEBİ N., EKEN T. Y.

The International Journal of Energy and Engineering Sciences, cilt.1, sa.3, 2016 (Hakemli Dergi)